NEW!!! FLASH COPPER an Alkali Copper Plating System

Flash Copper

 

DOES THE IMPOSSIBLE - plates onto,

 

LEAD, POT METAL, STEEL, PEWTER, ZINC, BRASS, 

ZINCATED ALUMINUM, ELECTROLESS NICKEL, AND COPPER.

 

Must not be used with SilvaSpray

 

Eliminates the use of cyanide strike coats.

Eliminates the use of Pot Metal Primer on Zinc

Eliminates the use of Nickel Strike on Steel prior to copper plating

Ideal for priming the lead on fishing lures, and sun catchers, prior to plating with Nickel or Copy Chrome

Increases the bond of acid copper, nickel and Copy Chrome to all substrates

 

 

Ideal for ‘priming the lead on fishing lures, and sun catchers, prior to plating with Nickel or Copy Chrome Increases the bond of acid copper, nickel and Copy Chrome to all substrates. See our new FLASH COPPER PlugNPlate Kit

 

FLASH COPPER is a unique alkaline electrolytic copper plating process with covering and throwing powers greater than cyanide copper.  FLASH COPPER is an outstanding pre-plate copper strike for bright nickel, acid copper, tin and solder plates. It is an excellent heat treat stop off plate and EMI shield. It is also an excellent decorative finish for buttons, rivets, lighting fixtures and builders’ hardware. The copper plate can be readily blackened or oxidized for a variety of attractive antiqued finishes. There are no carbonates to be treated. It contains no strong chelators. It is supplied as a liquid concentrate, which is diluted with water. FLASH COPPER produces a fine grained, smooth, dense and ductile copper deposit, which is nonporous and has excellent bonding properties.

 

The throwing and covering power of the non-cyanide process is superior to cyanide processes. It has uniform low current density distribution with excellent micro-throw.  The grain is smaller than cyanide copper, which increases the density of the deposit. This density provides excellent heat treat stop off and masking properties. The fine-grained FLASH COPPER deposit under nickel/chrome improves the overall corrosion resistance and helps to throw the nickel farther into the low current density areas. FLASH COPPER produces a softer and more ductile deposit than cyanide or acid copper. The soft deposit imparts improved adhesion and corrosion resistance and greatly improved resistance to thermal shock.  It has a high deposit purity and hence no out-gassing with subsequent brazing, soldering or vacuum operations.

 

FLASH COPPER is simple and inexpensive to use because it replenishes the copper in solution by dissolving the copper anode and here again it is a unique product with only one maintenance additive. The kit contains PICKLE # 4, a new product that replaces the use of flouroboric acid for etching lead and solder. The pickle can also be used on most other metals.

 

FLASH COPPER Benefits

  • One solution serves as both a strike and a plate bath.

  • Greater throwing power than acid copper

  • Eliminates the inherent dangers of cyanide in the work place and improves employee health and safety.

  • FLASH COPPER has excellent bath stability and high efficiency. The bath does not have to be dumped as with other baths due to breakdown products or iron buildup.

  • The bath is easily maintained by monitoring the pH and copper metal concentration.

  • It has a very wide operating window.

  • FLASH COPPER is supplied as a liquid concentrate, which is diluted with distilled water.

 

The 1.5gal US (5.5 litres-) FLASH COPPER Kits contain:

 

FLASH COPPER Part A 2 quarts

FLASH COPPER Part B  1 pint

FLASH COPPER Part C  1 pint

1 Plating tank and lid - 6 litres,

2 Copper Anode 4 x 8,

1 Heater/ Thermostat unit 100w, (34oc)

1 x 1 kg SD Pickle # 4

1 x The Complete Plating Manual

 

PROD # FL1                    FLASH COPPER Kit 5.5 litres                            £168.00 plus p&p

 